助手标题
全文文献 工具书 数字 学术定义 翻译助手 学术趋势 更多
查询帮助
意见反馈
共[2]页 共[25]条 当前为第1条到20条
 

相关语句
hydrothermal ageing
The practical adhesion of maleic anhydride grafted polyethylene (MAH-PE) to galvanised steel was studied using 3-point flexure tests, before and after hydrothermal ageing.
      
Influence of hydrothermal ageing and thermal treatments on the viscoelastic behavior of DGEBA-MCDEA epoxy resin
      
Cellulose undergoing accelerated hydrothermal ageing gives a pattern of carbonyl groups whose vibrational modes were observed in UV/VI/NIR, FTIR and Raman spectra.
      
The examination of the tribological situation of AMC, especially under challenging condition of hydrothermal ageing, shows the aptitude of this material in wear applications.
      
Hydrothermal ageing of Fe-ZSM5 resulted in a small loss in NOxconversion and enhanced N2O formation.
      
Hydrothermal ageing of CSM-laminate during water immersion - an acousto-ultrasonic study
      
Studies of damage under hydrothermal ageing incurred by random fibre-reinforced laminates have been carried out with this technique.
      
Hydrothermal ageing of CSM-laminate during water immersion - an acousto-ultrasonic study
      
Studies of damage under hydrothermal ageing incurred by random fibre-reinforced laminates have been carried out with this technique.
      
Hydrothermal ageing of jute-glass fibre hybrid composites - an acousto-ultrasonic study
      
Studies of damage under hydrothermal ageing incurred by random fibre glass-reinforced laminates and jute-glass fibre hybrid composites have been carried out using an acoustoultrasonic technique.
      
Changes in the crystalline phase and microstructure resulting from hydrothermal ageing of Y-TZP, (Y,Ce)-TZP, Y-TZP-Al2O3 composites and (Y,Ce)-TZP-Al2O3 composites were investigated under hydrothermal conditions at 180 °C and 1 MPa.
      
(Y,Ce)-TZP-Al2O3 composites were resistant to phase transformation during hydrothermal ageing.
      
In addition, the effects of hydrothermal ageing on the conductivities of the ceramics were evaluated.
      
The effect of copper oxide on sintering, microstructure, mechanical properties and hydrothermal ageing of coated 2.5Y-TZP cerami
      
Copper oxide dopants in amounts up to 1 wt% were added to 2.5 mol% yttria-coated zirconia powders in studies of sintering, microstructure, mechanical properties and hydrothermal ageing behaviour.
      
Copper oxide additions aid low temperature sintering and offer potential for property enhancement with a particularly high toughness being measured as well as improving resistance to structural degradation in 180°C hydrothermal ageing.
      
Physico-chemical effects of hydrothermal ageing of sheet molding compounds between -60 and 250°C
      
The understanding of the hydrothermal ageing effects of this material is an important factor for its improvement, because this heterogeneous material very easily deteriorates in the presence of humidity.
      
Hydrothermal ageing of yttria-stabilised zirconia, sintered at 1300°C-1325°C: the effects of copper oxide doping and sintering t
      
 