  硬断
     It analyses the main reason of electrode hard breakage accident for 2 × 12. 5MVA Mn-Si furnace, puts forward available protection measures as well as the reason that is caused by faster charge exaltation after power sends again.
     分析了2×12.5 MVA锰硅合金电炉在长时间热停炉后发生电极硬断事故的主要原因,笔者认为是由于重新恢复送电后负荷提升速度过快造成,并提出了预防电极硬断的有效措施。
短句来源
     ANALYSIS AND PREVENTION OF ELECTRODE HARD BREAKAGE REASON OF HEAT BLOW-OFF
     热停炉电极硬断原因的分析与预防
短句来源
     The electrode hard breakage after lo ng time shut down of 50MVA FeSi furnace is analysed according with effect of electrode current changes on electrode paste properties and th ermal stress,and it is concluded that electrode hard breakage is because of not only paste quality,but also electrode current .
     针对50MVA硅铁电炉在长时间停炉后发生电极硬断的现象,分析了电极电流的变化对自焙电极电极糊性质和热应力的影响,从而得出电极硬断不仅是由电极糊的质量引起的,电极电流也决定了自焙电极的使用。
短句来源
     Electrode hard breakage incident rate and corresponding losses are decreased by adopting improved craft of power cut and send.
     采用改进停送电工艺后,减少了电极硬断事故率及相应的经济损失。
短句来源
  相似匹配句对
     The causes judgement of drawing breakage of hard wire
     硬线盘条拉拔断裂原因初步判断
短句来源
     Bone breakage
     老母鸡的骨折
短句来源
     Livelihood was hard;
     民生艰难,思想混乱。
短句来源
     hard liver;
     肝脏质地坚硬;
短句来源
     ANALYSIS AND PREVENTION OF ELECTRODE HARD BREAKAGE REASON OF HEAT BLOW-OFF
     热停炉电极硬断原因的分析与预防
短句来源
查询“hard breakage”译词为用户自定义的双语例句

    我想查看译文中含有:的双语例句
例句
没有找到相关例句


The electrode hard breakage after lo ng time shut down of 50MVA FeSi furnace is analysed according with effect of electrode current changes on electrode paste properties and th ermal stress,and it is concluded that electrode hard breakage is because of not only paste quality,but also electrode current .

针对50MVA硅铁电炉在长时间停炉后发生电极硬断的现象,分析了电极电流的变化对自焙电极电极糊性质和热应力的影响,从而得出电极硬断不仅是由电极糊的质量引起的,电极电流也决定了自焙电极的使用。

It introduces the practice of electrodes maintenance during the process of power cut and send for 12. 5MVA submerged arc furnace. Electrode hard breakage incident rate and corresponding losses are decreased by adopting improved craft of power cut and send.

介绍了12.5MVA矿热炉在停送电过程中电极维护的实践。采用改进停送电工艺后,减少了电极硬断事故率及相应的经济损失。

It analyses the main reason of electrode hard breakage accident for 2 × 12. 5MVA Mn-Si furnace, puts forward available protection measures as well as the reason that is caused by faster charge exaltation after power sends again.

分析了2×12.5 MVA锰硅合金电炉在长时间热停炉后发生电极硬断事故的主要原因,笔者认为是由于重新恢复送电后负荷提升速度过快造成,并提出了预防电极硬断的有效措施。

 
图标索引 相关查询

 


 
CNKI小工具
在英文学术搜索中查有关hard breakage的内容
在知识搜索中查有关hard breakage的内容
在数字搜索中查有关hard breakage的内容
在概念知识元中查有关hard breakage的内容
在学术趋势中查有关hard breakage的内容
 
 

CNKI主页设CNKI翻译助手为主页 | 收藏CNKI翻译助手 | 广告服务 | 英文学术搜索
版权图标  2008 CNKI-中国知网
京ICP证040431号 互联网出版许可证 新出网证(京)字008号
北京市公安局海淀分局 备案号:110 1081725
版权图标 2008中国知网(cnki) 中国学术期刊(光盘版)电子杂志社